Pertambangan serat poliéster bolong kaku
Parameter
No. | Modél | Kakuatan regangan kN/m |
| ||
Bujur | melintang | Bujur | melintang | ||
1 | HG WP pepet R90-90MS | ≥90 | ≥90 | ≤10 | ≤10 |
2 | HG WP pepet-R110-110MS | ≥110 | ≥110 | ≤10 | ≤10 |
3 | HG WP pepet-R130-130MS | ≥130 | ≥130 | ≤10 | ≤10 |
4 | HG WP pepet-R170-170MS | ≥170 | ≥170 | ≤10 | ≤10 |
5 | HG WP pepet-R230-230MS | ≥230 | ≥230 | ≤10 | ≤10 |
6 | HG WP pepet-R270-270MS | ≥270 | ≥270 | ≤10 | ≤10 |
7 | HG WP pepet R330-330MS | ≥330 | ≥330 | ≤10 | ≤10 |
8 | HG WP pepet-R370-370MS | ≥370 | ≥370 | ≤10 | ≤10 |
9 | HG WP pepet-R430-430MS | ≥430 | ≥430 | ≤10 | ≤10 |
10 | HG WP pepet-R470-470MS | ≥470 | ≥470 | ≤10 | ≤10 |
11 | HG WP pepet-R530-530MS | ≥530 | ≥530 | ≤10 | ≤10 |
12 | HG WP pepet-R630-630MS | ≥630 | ≥630 | ≤10 | ≤10 |
13 | HG WP pepet-R730-730MS | ≥730 | ≥730 | ≤10 | ≤10 |